Page 1 of 1

Drool you bishes

Posted: July 22nd, 2006, 3:30 pm
by mongo
Image
Image

Drool you bishes

Posted: July 22nd, 2006, 3:50 pm
by tunnelrat
Very nice! What did that cost and where did you have it done?

Drool you bishes

Posted: July 22nd, 2006, 4:45 pm
by mongo
$85 here in texas

Sledgehammer Arms / Randy Kline (FAL files)

Manganese Phosphate finish.

Drool you bishes

Posted: July 22nd, 2006, 5:05 pm
by mongo
Here's a better pic of the finish
Image

Drool you bishes

Posted: July 22nd, 2006, 7:38 pm
by pshootr
Is that what's known as "Parkerizing"?
PshootR

Drool you bishes

Posted: July 22nd, 2006, 11:13 pm
by mongo
Is that what's known as "Parkerizing"?
PshootR
yes.

the slide on the P-64 is so farkin hard that Manganese Phosphate is the only parking that will hold.

But it holds well.

I soaked it in Remoil and wiped down the excess and I will guarantee you it will hold up better than most moly coatings and won't crack or chip.

Drool you bishes

Posted: July 23rd, 2006, 10:03 am
by abwehr
mongo,

I was finally able to see the photos, and I LIKE IT! A good parkerized finish is one of the best to me. There are a number of "shades" with parkerizing from the light grey to an almost black finish. The color has to do with the type parkerizing solution.

This finish really holds oil well and resist rusting. This is the type finish used on many military arms that hold up well. GREAT LOOKING PISTOL